Renewable Energy

Emulsion buffer layer limits screen-printing damage in copper-plated HJT solar cells

Chinese researchers link efficiency loss to worn screen mesh knuckles and find that a 4.7% emulsion coverage offers the best protection-uniformity trade-off.

Signe HalvorsenNovember 15, 20265 min read0 views
A conceptual close-up of a screen-printing mesh above a solar cell wafer, with an emulsion buffer layer separating the mesh from the cell surface.

Researchers in China have investigated how screen printing degrades copper-plated silicon heterojunction (HJT) solar cells and have proposed a modified screen design intended to reduce the damage. The work focuses on the photoresist-printing step used in copper plating, where the screen comes into direct contact with the wafer across a much larger area than in conventional silver-paste printing.

Screen printing is a standard metallization technique, but its mechanical pressure and thermal treatments can harm the passivating contact structures that are central to HJT performance. Such damage raises recombination losses and lowers conversion efficiency. The problem is especially important for copper-plated HJT cells, which are being pursued as a way to cut metallization costs and reduce dependence on silver.

Why photoresist printing is different

Corresponding author Lang Zhou explained that the screen-printing process for photoresist in HJT cells differs fundamentally from silver-paste printing. In silver printing, screen openings occupy only 2–5% of the total area, while an emulsion layer covers the rest and prevents the mesh from touching the wafer. Full-area photoresist coating, by contrast, typically uses a screen without emulsion coverage so that resist can be deposited uniformly across the wafer. As a result, the mesh makes direct and extensive contact with the wafer during every printing cycle.

Previous investigations cited by the researchers found that conversion efficiency fell from 26.2% to 25.7% over 15,000 consecutive printing cycles in commercial solar cell production. The losses were mainly in open-circuit voltage and fill factor, while short-circuit current density and electrical resistance remained largely unchanged. Minority carrier lifetime degradation rose from 0.61% with a new screen to 11.0% after 15,000 cycles.

Wear at the mesh knuckles

Using three-dimensional confocal microscopy, the team identified progressive wear of the screen mesh knuckles as the main cause. As the knuckles wore down, their contact area with the wafer grew, increasing mechanical stress on the underlying passivation layers. Scanning electron microscopy showed no visible surface scratches, but photoluminescence measurements indicated higher recombination losses. The researchers say this points to damage at the sensitive amorphous silicon/crystalline silicon interface.

To address the problem, they developed an emulsion buffer layer designed to keep the screen mesh from touching the wafer surface. They evaluated six patterns with emulsion coverage ratios from 2.9% to 16.6%.

Protection versus coating uniformity

The results revealed a trade-off. Higher emulsion coverage reduced mechanical damage but impaired photoresist distribution and coating uniformity. A coverage ratio of 4.7% provided the best balance, limiting minority carrier lifetime degradation to 0.41% after 10,000 printing cycles while maintaining relatively good coating uniformity. The researchers attribute the improvement to the emulsion layer preventing direct contact between the mesh and the wafer, thereby reducing cumulative mechanical damage to the passivation layers.

Zhou said the findings show that a relatively simple modification to screen design can substantially mitigate printing-induced degradation, offering a practical route to improving manufacturing reliability for copper-plated HJT cells. The results were published in Solar Energy in a paper on screen-printing photoresist-induced efficiency degradation and mitigation in Cu-plated SHJ solar cells.

Copper metallization momentum

The work comes as copper metallization attracts growing interest as an alternative to silver contacts in HJT cells. In April 2026, researchers at China’s Nankai University reported a silver-free HJT cell with 25.2% efficiency using plasma-induced interface engineering and copper electroplating. That approach addressed adhesion, contact resistance and stability challenges at the indium tin oxide interface.

Separately, scientists at Germany’s Forschungszentrum Jülich achieved 23.08% efficiency in a fully copper-metallized HJT cell. The silver-free device showed a relatively small efficiency penalty compared with its silver-metallized counterpart, while cells combining silver-copper paste on the front and silver contacts on the rear reached 23.95%. The results underline copper’s potential to reduce silver consumption, while further improvements in processing and electrical performance are still needed.